Portland Cement with Untreated Silica Fume and Silane
Subcategory: Concrete
Close Analogs: This data comes from a study that examined the effect of silica fume on Portland cement pastes. A total of four data sheets are in MatWeb from this study.
Material Notes: Portland cement (Type I) paste with no aggregate prepared with a water/cement ratio of 0.35:1 and cured 28 days. 15 wt% silica fume added; mean particle size 0.1 to 0.2 micron. Silane coupling agent admixture (0.2%) was aqueous amino vinyl silane (Hydrosil 2781).
| Available Properties |
- Density
- Porosity
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Compressive Strength
- Compressive Modulus
- Specific Heat Capacity
- Thermal Conductivity
- Shrinkage
|
|
|
|
| Property Data |