Mid-Mountain Materials Siltex® 10 Amorphous Silica Textile
Subcategory: Glass; Oxide, Silicon; Glass Fiber; Oxide; Composite Fibers
Material Notes: Description: Siltex® is a family of high performance textile fabric that is comprised of high purity, high strength amorphous silica fibers that are woven into a strong, flexible fabric designed for use where severe temperature conditions exist. SILTEX is excellent for protection of personnel and equipment against welding splatter, sparks, grinding of metals, etc. SILTEX is also excellent for use in engineered thermal insulation systems designed for severe temperatures – areas such as Turbine Covers, Exhaust Silencer Covers, etc. The amorphous silica fibers that make up SILTEX are unaffected by most chemicals, except strong alkalis, hydrofluoric acid or sodium. All SILTEX fabrics are available in standard and pre-shrunk (fired) versions, and are available with several coating and treatment options that enhance certain properties of the product in order to meet required performance characteristics. Information provided by Mid-Mountain Materials.
| Available Properties |
- Density
- Thickness
- Abrasion
- Melting Point
- Maximum Service Temperature, Air
- Shrinkage
- Break Strength
- Color
- Construction
- Material
- Packaging
- Tear Strength
- Width, standard
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|