Mid-Mountain Materials Padmat® MT1000 Needled Fiberglass Mat
Subcategory: Glass; Glass Fiber; Composite Fibers
Material Notes: Description: PADMAT® MT1000 fiberglass mat is comprised of high purity, high strength E-Glass fibers. These long fibers are mechanically needled into high strength, binderless insulation materials that are available in a wide range of thicknesses. MT1000 is light weight, strong, and highly efficient as insulation in most high heat environments for extended periods at elevated. The absence of organic or synthetic binders makes this product smoke free on heat up and allows the product to remain mechanically stable even after exposure to extreme temperatures. Characteristics: - Non combustible
- Good drapability
- Will not contribute to metal corrosion
- Will not decay, not sustain mold or vermin
- Excellent vibration resistance
- Odorless - will not absorb odors
- Excellent sound absorption qualities
- Flame spread / smoke generated - 0/0
Information provided by Mid-Mountain Materials.
| Available Properties |
- Density
- Thickness
- Thermal Conductivity
- Melting Point
- Maximum Service Temperature, Air
- Construction
- Material
- Width
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|