Mid-Mountain Materials Cermex™ PR 2200 High Temperature Paper
Subcategory: Glass; Glass Fiber; Composite Fibers
Material Notes: Description: High purity fiberglass, mineral wool and CMS (calcium-magnesium-silicate) fiber papers blended with organic and inorganic binders are capable of resisting heat up to 2300-1260. CERMEX™ HIGH TEMPERATURE PAPERS have superior thermal stability and easy handling properties before and after firing. Information provided by Mid-Mountain Materials.