Mid-Mountain Materials Thermoseal® Fiberpak® M100 Moldable

 

Subcategory: Ceramic/Metallic Coating; Ceramic

Material Notes:
Description: A family of high temperature moldables designed for a wide variety of uses. THERMOSEAL® FIBERPAK® MOLDABLES may be formed into shapes or linings, pushed into cracks and holes, or spread into thin sections as coating and separating mediums.

APPLICATION: THERMOSEAL® FIBERPAK® MOLDABLES are applied with the fingers, towels, spatulas, or from caulking guns. Gloves should be worn when hand applying. THERMOSEAL® FIBERPAK® MOLDABLES are easily formed to any contour or readily pressed into cracks and smoothed out. Water wet the tool to facilitate smoothing and contouring. Drying consists of removing the liquid portion of the mix usually by use of an external heat source at 220-200ºF • 95-150ºC for approximately six hours per inch of thickness.

USES:

  • Trough linings for molten metal transfer
  • High temperature sealing and coating
  • Light weight refractory shape manufacture
  • Trough coating and patching
  • Furnace Patching

PACKAGING:

  • 11 oz. Caulking tubes
  • 32 oz. Caulking tubes
  • One Gallon Bucket
  • 5 Gallon Buckets
  • 55 Gallon Drums

Information provided by Mid-Mountain Materials.

Available Properties
  • Density
  • Solids Content
  • Maximum Service Temperature, Air
  • Shrinkage
  • Alumina
  • Appearance
  • Color
  • Description
  • Silica
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。