Minelco MagnaDense 4 Fine Aggregate

 

Subcategory: Oxide

Material Notes:
MagnaDense is a high grade natural aggregate, manufactured from the iron oxide Magnetite. With its high density MagnaDense is used as loose ballast or as aggregate to produce high quality, high density concrete. This heavy concrete is some 60 % heavier than normal concrete and is easily produced and placed using standard equipment.

Minelco is unique in having its own in-house resources guaranteeing a long term reliable supply of consistent quality products. MagnaDense grades can be tailor made to specific customer requirements or purchased as standard grades.

Having a high particle density MagnaDense offers several advantages:

  • Reduced volumes = less excavation, transportation, reinforcement & time
  • Increased weight for a given volume
  • Reduced heat of hydration
  • High submerged/saturated density
  • High radiation shielding characteristics
  • Space saving
  • Noise and vibration dampening
  • Thermal energy storage

Applications: MagnaDense has a long history of use as construction material for both in-situ and precast applications.Loose ballast:
  • Offshore ballasting of rigs and caissons
  • Scour protection for underwater structures of pipelines
  • Ground stabilisation - to reduce piling

Heavy concrete:
  • Under water concrete (tunnels, pipeline mattresses)
  • Counterweights (bridges, locks, sluices, elevators, excavators)
  • Coastal protection (breakwaters, precast antifer cubes)
  • Pipecoating (negative buoyancy coatings)
  • Radiation shielding (medical & nuclear)

MagnaDense is available in grades from 30 mm down to powder fineness, supplied from strategic stockpiles throughout Europe and the U.S.

The use of MagnaDense enhances the density of concrete. Full replacement of the local aggregate, both fine and coarse, makes it possible to reach a density of 4.0 t/m3, or interim densities by partial replacements.

Available Properties
  • Specific Gravity
  • Bulk Density
  • Water Absorption
  • Hardness, Mohs
  • Particle Shape
  • Surface texture
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。