3M Nextel™ 440 Industrial Ceramic Fiber
Subcategory: Oxide, Silicon; Oxide, Aluminum; Oxide; Composite Fibers
Key Words: Alumina, Aluminum Oxide
Material Notes: Chemical composition above is wt%. Crystal phases are gamma alumina + mullite + amorphous SiO2. Filament diameter is 10-12 µm. 3M Nextel fibers 312, 440, and 550 are designed for non-structural applications where their primary purpose is to act as a flame barrier. 3M Nextel Ceramic Fiber 440 is made from Al2O3, SiO2, and B2O3. Because B2O3 is present, this composition has both crystalline and glassy phases. The glassy phase helps the fiber retain strength after exposure to high temperatures because it slows the growth of crystalline phases that weaken the fiber. However, when the fiber is stressed at high temperature, the glassy phase weakens the fiber due to viscous flow much like a glass fiber. Information provided by 3M Ceramic Textile and Composites.
| Available Properties |
- Density
- Particle Size
- Specific Surface Area
- Tensile Strength, Ultimate
- Modulus of Elasticity
- Dielectric Constant
- Dissipation Factor
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Melting Point
- Refractive Index
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|