3M Nextel™ 550 Industrial Ceramic Fiber
Subcategory: Oxide, Silicon; Oxide, Aluminum; Oxide; Composite Fibers
Key Words: Alumina, Aluminum Oxide
Material Notes: Chemical composition above is wt%. Crystal phases are gamma alumina amorphous SiO2. Filament diameter is 10-12 µm. 3M Nextel fibers 312, 440, and 550 are designed for non-structural applications where their primary purpose is to act as a flame barrier. 3M Nextel Ceramic Fiber 550 is made from Al2O3, SiO2, and B2O3. Because 550 does not contain B2O3, this composition retains its strength better at high temperature. Information provided by 3M Ceramic Textile and Composites.
| Available Properties |
- Density
- Particle Size
- Specific Surface Area
- Tensile Strength, Ultimate
- Modulus of Elasticity
- Dielectric Constant
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Melting Point
- Refractive Index
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|