3M™ Scotchlite™ Glass Bubbles S60HS
Subcategory: Glass; Additive/Filler for Polymer
Material Notes: High-strength polymer additives made from a water-resistant and chemically-stable soda-lime-borosilicate glass. These hollow glass microspheres can be used as a low density filler material for plastic and rubber parts created from injection molding, extrusion processes and/or other vigorous process equipment (Banbury mixers, etc.) Scotchlite glass bubbles help to reduce weight, improve abrasion resistance, reduce thermal expansion, increase surface hardness and contribute to cost savings. They are used as additive materials in the automotive, truck, rail and aerospace industries. Information supplied by 3M Specialty Materials.
| Available Properties |
- Density
- Bulk Factor
- Loss On Ignition
- Particle Size
- pH
- Compressive Strength
- Softening Point
- Alkalinity
- Color, Unaided Eye
- Composition
- Flotation (density<1.0 g/cc)
- Oil Absorption
- Shape
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|