Morgan Advanced Ceramics Deranox™ 975 Alumina
Subcategory: Oxide, Aluminum; Oxide
Key Words: Al2O3; Aluminum Oxide
Material Notes: Fine grain alumina ceramic of 97.5% Al2O3 content. A high quality material, widely used for electrical and mechanical components that require thick film metallizing, as well as for dynamic duties where resistance to abrasion and chemical attack are essential. Prime features: - Can be thick film metallized with noble metals
- High volume resistivity
- High mechanical strength
- Excellent corrosion resistance
- Excellent wear resistance
- Low coefficient of friction
- High thermal stability
- High density, non-porous and vacuum tight
Typical applications:- Thick film metallized components, such as those with conductor and/or resistor networks, dielectric layers, solderable interfaces, etc
- High-integrity devices for duties in the defense, aerospace, medical, laser and scientific instrument fields
- Dynamic and static components in pumps and valves that handle corrosive or abrasive media.
Information provided by Morgan Advanced Ceramics.
Available Properties |
- Density
- Porosity
- Particle Size
- Hardness, Rockwell 45 N
- Vickers Microhardness
- Modulus of Elasticity
- Flexural Strength
- Compressive Strength
- Fracture Toughness
- Electrical Resistivity at Elevated Temperature
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- CTE, linear 500°C
- Specific Heat Capacity
- Thermal Conductivity
- Maximum Service Temperature, Air
- Color
- Thermal Downshock
|
|
|
|
Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|