Morgan Advanced Ceramics Deranox™ 995 Alumina

 

Subcategory: Oxide, Aluminum; Oxide

Key Words: Al2O3; Aluminum Oxide

Material Notes:
Alumina ceramic of 99.5% Al2O3 content. This material is extensively used for applications that require exceptional electrical resistance combined with resistance to chemical attack.

Prime features:

  • Ultra-low outgassing
  • Low neutron absorption
  • Resistant to fluorine and chlorine attack
  • Very high volume resistivity
  • Good thermal conductivity
  • Non-porous and vacuum tight.
Typical applications:
  • Gas, solid-state and waveguide lasers
  • Components for a wide range of industrial, medical and defense equipment.

Information provided by Morgan Advanced Ceramics.

Available Properties
  • Density
  • Porosity
  • Particle Size
  • Hardness, Rockwell 45 N
  • Vickers Microhardness
  • Modulus of Elasticity
  • Flexural Strength
  • Compressive Strength
  • Electrical Resistivity at Elevated Temperature
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor
  • CTE, linear 500°C
  • Specific Heat Capacity
  • Thermal Conductivity
  • Thermal Conductivity at Elevated Temperature
  • Maximum Service Temperature, Air
  • Color
  • Thermal Downshock
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。