Morgan Advanced Ceramics Sintox™ FF Alumina
Subcategory: Oxide, Aluminum; Oxide
Key Words: Al2O3; Aluminum Oxide
Material Notes: Alumina ceramic with a minimum Al2O3 content of 95.0% (typically 96%). This material is a high quality electrical insulator, with good mechanical properties, that is widely used for components in consumer products as well as for high integrity applications. Prime features: - High volume resistivity
- Low coefficient of expansion
- Dense, non-porous and vacuum tight
- Resists abrasive wear and chemical attack
- Fire resistant and non-outgassing
Typical applications:- Laser power tubes
- Telecommunications components
- Aerospace components
- Automobile components
- Domestic product components
- Process equipment components
Information provided by Morgan Advanced Ceramics.
| Available Properties |
- Density
- Porosity
- Particle Size
- Hardness, Rockwell 45 N
- Vickers Microhardness
- Modulus of Elasticity
- Flexural Strength
- Compressive Strength
- Fracture Toughness
- Electrical Resistivity at Elevated Temperature
- Dielectric Constant
- Dissipation Factor
- CTE, linear 500°C
- Thermal Conductivity
- Color
- Sonic Velocity
- Thermal Downshock
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|