Murlin Natural Bone Ash Mold Release
Subcategory: Ceramic; Adhesives, Sealants, and Coatings
Material Notes: Description: Bone ash is used as a mold release agent. Information provided by Murlin Chemical, Inc.
| Available Properties |
- Density
- Loss On Ignition
- Ash
- CaO
- CO2
- Color
- MgO
- P2O5
- Screen
- SiO2
|
|
|
|
| Property Data |