Mykroy/Mycalex 1600 Machining Grade Glass-bonded Mica Composite
Subcategory: Glass; Glass Ceramic
Material Notes: Mykroy/Mycalex 1600 is a compression molded glass mica composite that is the perfect alternative to high performance plastics where high temperature, good dielectric strength and good arc resistance are required. This material is softer than other high temperature machinable ceramics allowing for the fabrication of intricate or complex shapes. It can be drilled or tapped and can accommodate helical inserts. In addition, no post firing is required after fabrication. Product Benefits: - Higher operating temperature
- Exceptional dimensional stability
- High compressive strength
- Higher thermal shock resistance
- Completely inorganic
- Does not burn or outgas
- Impervious to moisture, oils, and gases
- Withstands thermal cycling
- Low thermal conductivity
- High dielectric strength
- Low electrical loss
- High arc resistance
- Vacuum tight
- Can be glued with epoxy, sealing glass, or ceramic adhesives
Glass bonded mica specification ASTM D1049.Typical data below provided by Mykroy/Mycalex Ceramics.
| Available Properties |
- Density
- Water Absorption
- Hardness, Rockwell A
- Hardness, Rockwell H
- Tensile Strength @ Break
- Modulus of Elasticity
- Flexural Strength
- Compressive Strength
- Izod Impact, Notched
- Volume Resistivity
- Surface Resistivity per Square
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Dielectric Loss Index
- Arc Resistance
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Thermal Conductivity
- Maximum Service Temperature, Air
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|