NanoScale® NanoActive® Aluminum Oxide
Subcategory: Oxide, Aluminum; Oxide
Close Analogs: Composition based on metal
Material Notes: NanoActive Al2O3 is produced using proprietary processes to obtain high specific surface area, low density, amorphous material with high adsorption capacity and chemical reactivity. NanoActive Al2O3 can be dispersed in various carrier fluids with greatly reduced particle sizes.Applications: Applications include air cleaning, capacitors, catalysts supports, coatings, heat transfer fluids (suspensions), polishing materials, polymer nanocomposites for improved tribological performance, and structural ceramics. Information provided by NanoScale
| Available Properties |
- Density
- Bulk Density
- Loss On Ignition
- Particle Size
- Specific Surface Area
- Pore Size
- Appearce / Color
- Crystallite Size
- Minimum Total Pore Volume cc/g
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|