NanoScale® NanoActive® Calcium Oxide Plus
Subcategory: Oxide, Other; Oxide
Close Analogs: Composition based on metal
Material Notes: NanoActive CaO Plus is produced using proprietary processes to obtain high specific surface area (over 90 m²/g vs. 1-2 m²/g for standard CaO), small crystallite size material possessing high chemical reactivity towards many chemical hazards including carbon dioxide and hydrogen sulfide.Applications: Applications include desiccant, destruction of chemical warfare agents, elevated temperature hazardous waste treatment, flue gas treatment, insecticide and fungicide, odor reduction, precursor, pulp and paper, and water treatment. Information provided by NanoScale
| Available Properties |
- Density
- Bulk Density
- Particle Size
- Specific Surface Area
- Pore Size
- Appearce / Color
- Crystallite Size
- Minimum Total Pore Volume cc/g
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|