NanoScale® NanoActive® Cerium Oxide

 

Subcategory: Oxide, Other; Oxide

Close Analogs: Composition based on metal

Material Notes:
NanoActive CeO2 is produced using proprietary processes to obtain high specific surface area, aggregated dry powder that can be dispersed in various carrier fluids to significantly reduce the particle size.

Applications: Applications include catalysts, enhancement of Near IR reflection, industrial coatings, polishing slurries, and reactive dopants.

Information provided by NanoScale

Available Properties
  • Density
  • Bulk Density
  • Loss On Ignition
  • Particle Size
  • Specific Surface Area
  • Pore Size
  • Moisture Content
  • Appearce / Color
  • Crystallite Size
  • Minimum Total Pore Volume cc/g
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。