NanoScale® NanoActive® Titanium Dioxide
Subcategory: Oxide, Titanium; Oxide
Close Analogs: Composition based on metal
Material Notes: NanoActive TiO2 is produced using proprietary processes to obtain high specific surface area (over 500 m²/g), high porosity, weakly aggregated, amorphous material possessing extraordinary adsorption capacity and chemical reactivity.Applications: Applications include catalysts and catalyst supports, cosmetic and skin care market, destruction of chemical warfare agents, paints and coatings, protective apparel and personal protection equipment, smoke removal, structural ceramics, and UV protecting clear coats. Information provided by NanoScale
| Available Properties |
- Density
- Bulk Density
- Loss On Ignition
- Particle Size
- Specific Surface Area
- Pore Size
- Moisture Content
- Appearce / Color
- Crystallite Size
- Minimum Total Pore Volume cc/g
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|