NanoScale® FAST-ACT® Formulation RNP-212
Material Notes: The FAST-ACT family of products was designed to offer protection against that "once in a lifetime" response to a Chemical Warfare Agent, while at the same time offering a single highly effective solution to deal with more common release such as hydrofluoric acid or pesticides. FAST-ACT enables the use of a single product to mitigate threats posed by highly toxic chemicals in either liquid or vapor form.Applications: Information provided by NanoScale
| Available Properties |
- Bulk Density
- Loss On Ignition
- Particle Size
- pH
- Specific Surface Area
- Moisture Content
- Appearce / Color
|
|
|
|