NAPCO C85 - RK Bauxite
Subcategory: Oxide, Aluminum; Oxide
Key Words: Chinese shaft kiln bauxites, aluminum hydroxides
Material Notes: Round kiln calcined low alkali refractory grade bauxite form the Shanxi province of China. Its high alumina content and high density make it an ideal refractory aggregate for certain castables and specialties. Data provided by the manufacturer, North American Processing Company.
| Available Properties |
|
We're sorry, but our sources do not report any other information for this material.
|
|
|
|