Pyrotek L-6 Fiberseal Blanket
Material Notes: Lightweight, yet strong and durable needled blankets. Dimensions 610 mm x 7.6 m 1219 mm x 7.6 m 6 - 51 mm thick Applications - Furnace linings
- Gaskets
- Expansion joints
- Fire blanket
- Fire pillows
Information provided by Pyrotek.
| Available Properties |
- Density
- Maximum Service Temperature, Air
|
|
|
|