Pyrotek M-4 Fiberseal Blanket
Material Notes: A white high-temperature felt. Dimensions 610 mm x 15.2 m 25 mm thick Applications - Gaskets
- Trough covers
- Trough gaskets
Information provided by Pyrotek.