Pyrotek M-9 Fiberseal Blanket
Material Notes: Maxsil ceramic-free insulation with excellent chemical resistance. Shot free. Dimensions 889 mm x 24.4 m x 13 mm 889 mm x 11.9 m x 25 mm Applications Information provided by Pyrotek.