Pyrotek SL-6 Fiberseal Blanket
Material Notes: A more consistently thick, rigid, dense and insulating version of M-6. Dimensions 610 mm x 15.2 m x 6 mm 1219 mm x 15.2 m x 6 mm 610 mm x 30.4 m x 12 mm 1219 mm x 30.4 m x 12 mm Applications - Die-cutting, fabrication and handling
- High purity fibers with excellent vibration resistance for aerospace insulation
Information provided by Pyrotek.
| Available Properties |
- Density
- Maximum Service Temperature, Air
|
|
|
|