Pyrotek T-1 Low-Temperature Felt
Material Notes: A dark brown, very strong and tough material. Dimensions 610 mm x 30.5 m 6 mm thick Applications - High-temperature reusable gaskets
Information provided by Pyrotek.
| Available Properties |
- Density
- Maximum Service Temperature, Air
|
|
|
|
| Property Data |