Pyrotek Pyloric 100 High-Temperature Product for Cooking Ovens
Material Notes: Pyrorock 100 is a refractory material used as a thermal transfer media in deck-type cooking ovens. Using our patented Isomag® process, mineral materials are combined with an inorganic binder. This unique formulation gives Pyrorock 100 durability, outstanding thermal transfer properties, excellent strength and thermal shock resistance. All this adds up to higher cooking productivity. Pyrorock is totally free of asbestos and free-silica and is easily cut to finished dimensions. Advantages - Durable
- Asbestos-free
- Promotes even temperature distribution on cooking deck
- Increases cooking consistency
- Improves wear characteristics
- Excellent thermal shock resistance
- Hard, tough chip resistant surface
Information provided by Pyrotek.
| Available Properties |
- Density
- Modulus of Rupture
- Flexural Strength
- CTE, linear 20°C
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|