Pyrotek Dry-Barrier Mix Dry Cathode Barrier Material
Material Notes: In the presence of cryolite, Dri-Barrier Mix is designed to form a viscous layer on its surface which prevents further penetration. The freezing isotherm sustained in Dri-Barrier Mix decreases the attack on the other insulating materials. Applications - Firebrick replacement
- Bedding material
- Sealant for collector bars
Advantages - Reduced cryolite consumption
- Easily installed in any cathode design
- Non wetting
- Reduces bottom shell temperature
- No joints or cracks
- No curing time
- No bedding mix required
- Minimizes chemical attacks on insulating materials beneath mix
- No steam evolution through the monolithic area
Information provided by Pyrotek.
| Available Properties |
- Thermal Conductivity at Elevated Temperature
- Shrinkage
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|