Pyrotek Pyrite N-17 Refractory Board
Subcategory: Oxide, Silicon; Oxide
Material Notes: Pyrotek N-17 is a graphite fiber reinforced, high purity, calcium silicate board developed exclusively for the non-ferrous casting industry. The patented formulation of Pyrotek N-17 makes it unparalleled in strength, low shrinkage and resistance to thermal shock. Our machine shops are equipped with CNC tooling equipment to produce complex components to customer specifications. Applications - Transition plates
- Continuous caster tips
- Baffle plates
- Trough liners
- Floats
- Machined spouts
- Head boxes
Advantages - Asbestos-free
- Low thermal conductivity
- Resistant to thermal shock
- Non-wetting
- Good machining characteristics
Information provided by Pyrotek.
Available Properties |
- Density
- Loss On Ignition
- Modulus of Rupture
- Compressive Strength
- CTE, linear 20°C
- Thermal Conductivity at Elevated Temperature
- Maximum Service Temperature, Air
- Shrinkage
- Screw Grip (Pull) Penetration Depth
|
|
|
|
Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|