Pyrotek Pyrocast PT-190 Refractory Cast Parts
Subcategory: Oxide, Aluminum; Oxide
Material Notes: Pyrocast PT-190 is an extremely dense alumina based refractory. It is best suited for applications where high velocity metal erosion potential is a problem, due to its strength and abrasion resistant characteristics. Pyrocast PT-190 also provides excellent hot load strength. Pyrocast PT-190 is frequently used for applications such as launders, tap out and burner blocks, and door blades. Information provided by Pyrotek.
| Available Properties |
- Density
- Modulus of Rupture
- Flexural Strength
- Compressive Strength
- Thermal Conductivity at Elevated Temperature
- Maximum Service Temperature, Air
- Shrinkage
|
|
|
|
| Property Data |