Pyrotek M-14 Compressible/Insulating Boards
Subcategory: Oxide, Silicon; Oxide, Aluminum; Oxide
Material Notes:
Applications - Siphon gaskets
- Trough and ladle linings
- Tundishes
- Mill board substitute
Advantages - Resistant to chemical attack
- Excellent thermal shock resistance
- Slightly flexible
- Moderately compressible
Information provided by Pyrotek.
| Available Properties |
- Density
- Loss On Ignition
- Modulus of Rupture
- Compressive Strength
- Thermal Conductivity at Elevated Temperature
- Maximum Service Temperature, Air
|
|
|
|