Pyrotek M-18 Compressible/Insulating Boards
Subcategory: Oxide, Silicon; Oxide, Aluminum; Oxide
Material Notes:
Applications - Trough, ladle and launder linings
- High temperature gaskets
- Mill board substitute
Advantages - Water moldable
- Excellent thermal shock resistance
- High compressibility
- Excellent resistance to chemical attack
Information provided by Pyrotek.
| Available Properties |
- Density
- Loss On Ignition
- Modulus of Rupture
- Thermal Conductivity at Elevated Temperature
- Maximum Service Temperature, Air
|
|
|
|