Pyrotek Pyrocast SC-2600 Castable Refractory
Subcategory: Carbide
Material Notes: Pyrocast SC-2600 is a high purity silicon carbide based refractory for applications requiring high thermal conductivity, resistance to metal and flame abrasion. Applications - Filter boxes
- Burner tubes
- Troughs
- Tap out blocks
- Special refractory shapes
- Baffles
- Filter bowl tiles
Advantages - Resistant to metal
- Resistant to flame abrasion
- High thermal conductivity
- Withstands high temperatures
- Extremely hard
Information provided by Pyrotek.