Pyrotek S-679 Dense Graphite Material Treated for Oxidation Resistance
Subcategory: Graphite; Carbon
Material Notes: S-679 is an isostatically pressed graphite material that is treated to provide oxidation resistance at elevated temperatures. This material performs well in glass contact applications where heat and abrasion cause other materials to fail. Applications - Take out tongs
- Dead plates
- Sweep out inserts
- Stacker bar covers
- Conveyor guides
- Transfer units
- Precision machined parts
- Rollers
Advantages - Asbestos-free
- Uniform heat distribution
- Non-sticking to glass
- Low heat capacity
- Long life
- Compatible in combination with steel or other metals
Information provided by Pyrotek.
| Available Properties |
- Density
- Flexural Strength
- Compressive Strength
- CTE, linear 20°C
- Thermal Conductivity
- Maximum Service Temperature, Air
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|