Pyrotek N-20T Compressible Insulation Board
Material Notes: Excellent characteristics allow for the manufacture of a very durable, smooth, hard roll surface which is non-marking to glass. Works well when a high temperature compressible gasket is required. Applications - Lehr rolls
- Gaskets
- Heat shields
Advantages - Excellent resistance to glass cullet abrasion
- Excellent thermal stability at elevated temperatures
- Superior surface hardness
- Minimal dusting
- Shot free
Information provided by Pyrotek.