Pyrotek Fiber Seal Y-1 Ceramic fiber paper
Subcategory: Oxide, Silicon; Oxide, Aluminum; Oxide
Material Notes: Y-1 Fiberseal paper is a light-weight refractory material. Y-1 is resistant to most chemicals with the exception of hydrofluoric and phosphoric acids and strong alkalis. Applications - Gaskets
- Seals
- Spacer material
Advantages - Temperature stability
- Low thermal conductivity
- Resilient
- Thermal shock resistant
- Easily shaped
- High heat reflectance
- Low heat storage
Information provided by Pyrotek.