Pyrotek A-1 Glass Fiber Core Rope
Subcategory: Glass
Material Notes: Compressible, inexpensive rope. Glass fiber core with heavy gauge glass fabric jacket. Loses tensile strength after 340°C but remains intact. Advantages - Good Abrasion Resistance
- Good Compression and Recall
Information provided by Pyrotek.
| Available Properties |
- Density
- Maximum Service Temperature, Air
|
|
|
|
| Property Data |