Pyrotek A-1/Z-5 Tadpoles
Subcategory: Glass
Material Notes: A-1 rope core with jacket and mounting flange of densely woven glass cloth or wire reinforced glass cloth. Advantages - Good Abrasion Resistance
- Good Compression and Recall
Information provided by Pyrotek.