Pyrotek Pyrocast PT-60 Castable Refractory
Subcategory: Oxide, Aluminum; Oxide
Material Notes: Pyrocast PT-60 is a ceramic fiber based insulating castable with very low thermal conductivity and excellent resistance to thermal shock. Applications - Launder linings
- Distributor pan linings
- Ladle linings
Advantages - In situ casting
- Excellent insulation characteristics
- Does not require pre-heating
Information provided by Pyrotek.