Pyrotek Fiberseal Paper C-6 Ceramic fiber paper
Material Notes: C-6 is an economical, high strength, Fiberseal paper composed of ceramic fibers, inert fillers and fiberglass. Applications Advantages - Low shrinkage
- Good dielectric properties
- Uniform thermal conductivity
- Easily shaped
- Low-cost
Information provided by Pyrotek.
| Available Properties |
- Density
- Binder
- Dielectric Strength
- Maximum Service Temperature, Air
|
|
|
|