Pyrotek Pyrocast TG Castable Refractory
Subcategory: Oxide, Silicon; Oxide
Material Notes: Pyrocast TG is a technical-grade silica based refractory developed for the non-ferrous industry including nickel, copper, zinc, and their alloys. Applications - Coreless induction furnace lining
- Channel-type furnace lining
- Kilns
- Boilers
- Heat treating furnaces
- Forge furnaces
- Copper base alloys
Advantages - Excellent thermal shock resistance
- Dimensionally stable
- Good insulation for density
- Does not inhibit induction energy transfer
Information provided by Pyrotek.
| Available Properties |
- Density
- Modulus of Rupture
- Compressive Strength
- CTE, linear 20°C
- Thermal Conductivity at Elevated Temperature
- Maximum Service Temperature, Air
- Shrinkage
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|