Pyrotek Pyrocast ICL Castable Refractory
Subcategory: Oxide, Silicon; Oxide, Aluminum; Oxide
Material Notes: Pyrocast ICL was developed exclusively for the induction furnace market as a coil lining refractory. This silica and alumina based material displays high strength and excellent thermal shock resistance. Applications - Induction coil lining
- Biller preheater lining
- Component linings
Advantages - Excellent window for induction energy
- Extremely stable
- Thermal shock resistant
- Minimum maintenance
- Resilient to cracking
- Fewest shorts
- Long-life coil lining
Information provided by Pyrotek.
| Available Properties |
- Density
- Modulus of Rupture
- Compressive Strength
- CTE, linear 20°C
- Thermal Conductivity at Elevated Temperature
- Maximum Service Temperature, Air
- Shrinkage
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|