Pyrotek MT-29P Microporous Panel Insulation
Material Notes: MT-29P is a unique panel insulation which offers exceptionally low thermal conductivity. The exterior of the panel is a glass fabric which maximizes the strength of the rigid interior panel. Applications Backup insulation for: - Troughs
- Filter bowls
- Furnace linings
- Transfer crucibles
- Door insulation
Advantages - Low thermal conductivity
- Reduces warping of vessels and troughing
- Promotes greater temperature control
- Minimizes heat transfer
- Can be designed to be reused
- Minimizes hot face temperature of vessels
- Provides low shrinkage at high temperatures
- Not wet by molten aluminum
Information provided by Pyrotek.
| Available Properties |
- Density
- Compressive Strength
- Thermal Conductivity at Elevated Temperature
- Maximum Service Temperature, Air
- Shrinkage
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|