Pyrotek MCX-40 Insulating Board
Material Notes: MCX-40 is a bonded-mica composite for use in glass contact applications. Its high operating temperature, low porosity, and low thermal conductivity make it ideal for all areas of hot glass transfer, including takeout jaws/inserts, sweep out pads, lehr loader bar pads/inserts, and high temperature flat glass quench rollers. Applications - Glass contact insulating material
Advantages - Abrasion resistant
- Non-marking to glass
- Low porosity
- Resists oxidizing atmospheres better than carbon or graphite
- Machinable with standard equipment
- High-impact strength
- Can be molded to net shape based on consumer specifications
Information provided by Pyrotek.
| Available Properties |
- Density
- Water Absorption
- Flexural Strength
- Compressive Strength
- Thermal Conductivity
- Maximum Service Temperature, Air
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|