Pyrotek Valcor® G Pre-Cast Shapes
Subcategory: Oxide, Aluminum; Oxide
Material Notes:
Applications - Burner blocks
- Skimmer blocks
- Cover blocks
- Specialty blocks
- Plungers
- Stirrers
- Spouts
- Feeder tubes
Advantages - Proven performance in molten glass contact applications
- Smooth surface finish does not mark or streak glass
- Molds readily available for most components
Information provided by Pyrotek.
| Available Properties |
- Density
- Open Porosity
- Permeability
- Modulus of Rupture
- CTE, linear 20°C
- Shrinkage
- Melt Temperature
|
|
|
|