Pyrotek ISOCAST Insulating Refractory Castable
Subcategory: Oxide, Silicon; Oxide
Material Notes: Pyrotek's Isocast is a refractory castable based on phosphate bonded calcium silicate material. Isocast exhibits excellent thermal insulation characteristics and very good behavior with respect to molten aluminum. Applications - Trough sections
- Hot-top table sections
- Launder lining
- Stub troughs
- Filter boxes
Advantages - Non-wetting
- Does not require preheating prior to usage
- Low K-factor
- Thermal shock resistant
- Non-asbestos
Information provided by Pyrotek.
| Available Properties |
- Density
- Modulus of Rupture
- Compressive Strength
- CTE, linear 20°C
- Thermal Conductivity
- Thermal Conductivity at Elevated Temperature
- Maximum Service Temperature, Air
- Shrinkage
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|