Pyrotek Pyrocast ALF2 Low Cement Refractory Castable
Subcategory: Oxide, Silicon; Oxide, Aluminum; Oxide
Material Notes: Pyrocast ALF2 is a low cement castable with mullite base. It is suited for applications requiring high strength at elevated temperatures and abrasion resistance. Applications - Aluminum melting and holding furnace linings
- Ladles
- Launders
- Degassing boxes
- De-mag boxes
Advantages - Outstanding hot strength
- High abrasion resistance
- Resistant to molten aluminum attack
Information provided by Pyrotek.
| Available Properties |
- Density
- Modulus of Rupture
- Thermal Conductivity at Elevated Temperature
- Maximum Service Temperature, Air
- Shrinkage
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|