Pyrotek Pyrocast XL Small Component Refractory
Subcategory: Oxide, Silicon; Oxide
Material Notes:
Applications - Thimbles
- Transition plates
- Down Spouts
- Control Pins
- Auto pour Ladles
- Strip Casting Nozzles
Advantages - Thermal shock resistance
- High erosion resistance
- High service temperature
- Smooth cast surface
- Dimensionally stable
- Preheating unnecessary
- Easily cleaned
- Non-wetting
Information provided by Pyrotek.