Pyrotek O'-Sialon Non-Oxide Ceramic
Subcategory: Carbide
Material Notes: O'-Sialon is a unique class of non-oxide ceramic which incorporates grains of silicon carbide held by a matrix of O'-Sialon. This results in a product that exhibits high strength at both room temperature and working temperature. It also gives longer life meaning less change-overs and less down time. No expensive and time consuming coatings are required because O'-Sialon is non-wetting to molten aluminum and its alloys. Applications - Dosing tubes
- Riser tubes
- Heater protection tubes
- Thermocouple Protection tubes
Advantages - Excellent oxidation resistance
- Non-wetting to aluminum and its alloys
- Good thermal shock
- Good abrasion resistance
- Chemically inert
Information provided by Pyrotek.
| Available Properties |
- Density
- Open Porosity
- Modulus of Rupture
- CTE, linear 20°C
- Thermal Conductivity at Elevated Temperature
- Maximum Service Temperature, Air
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|