Pyrotek Pyroslip 105 RFU High-Purity Graphite-Based Lubricant
Subcategory: Graphite; Carbon
Material Notes: Thick fluid consistency. Applications - Seamless steel pipe mandrel bar lubricant
- Aluminum extrusions billet and/or dummy block lubricant
- Hot steel closes die forging
Advantages - Environmentally friendly
- Nonflammable
- Noncombustible
Information provided by Pyrotek.