Pyrotek RFM Light density refractory composite material
Material Notes: The RFM material is a composite made of fiberglass fabric and a wollastonite slurry. It can be shaped to very complex and thin parts. It has a very good behavior against molten aluminum alloys. Applications - Distribution troughs for continuous casting machine
- Rigid molten metal distributor
- Float bottom part
- Casting tip
- Auto pour ladle
Advantages - No pre-heating required
- Excellent mechanical properties
- Excellent resistance to erosion
- Can be molded
- Non-wetting by molten aluminum
- High temperature service
Information provided by Pyrotek.
| Available Properties |
- Density
- Modulus of Rupture
- CTE, linear 20°C
- Thermal Conductivity at Elevated Temperature
- Maximum Service Temperature, Air
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|